May 21, 2006 #1 mali325 Materials Joined May 20, 2006 Messages 24 Location IR dear sirs -How can I remove fe from cu(consist of 5% fe). Best regards
May 21, 2006 #2 unclesyd Materials Joined Aug 21, 2002 Messages 9,819 Location US Comeback with more details of your problem. Upvote 0 Downvote
May 22, 2006 #3 NickE Materials Joined Jan 14, 2003 Messages 1,570 Location US Is there a mining/minerals processing/ore processing forum? Upvote 0 Downvote
May 22, 2006 Thread starter #4 mali325 Materials Joined May 20, 2006 Messages 24 Location IR Dear sirs Excuse me.The question was wrong. Question: As you know ,solution of fe in cu is difficult. How can I add fe to Al-boronz(17%Al)with 5% fe.(Cu-17Al-5%Fe). Best Regards Upvote 0 Downvote
Dear sirs Excuse me.The question was wrong. Question: As you know ,solution of fe in cu is difficult. How can I add fe to Al-boronz(17%Al)with 5% fe.(Cu-17Al-5%Fe). Best Regards