Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Burr removing from a H structural beam manufactured by induction welding

Status
Not open for further replies.

miguelandrade

Mechanical
Joined
Mar 28, 2013
Messages
26
Location
EC
Hello,

I am running a Thermatool HF Solid State Welder for structural beams (100x150mm to 200x460mm) at 12m/min. The output product does accomplish the joint strength code required, but it has a mild burr stuck on the beam web-flange joint.

When a client ask to remove the burr for aesthetic reasons, welders do it with an oxy-fuel equipment.

Does someone knows if the burr can be avoided by parameters regulation of the welding machine?

If it is not,a mechanical system and a control system associated to it has to be developed.

Does someone has experience dealing with this situation on structural sections manufactured using induction welding? Which solutions have you found? I already have some ideas on how to do it, but other's experience dealing with the same situation is a mine of ideas as well.

Thanks,

Miguel

 
This burr is from upspet material (squeezed out) correct?
Often a tool steel or carbide knife is used to skive off the burr.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
Yes, it is squeezed out to the surface because of the heat and pressure applied. This machining tool is placed on the hot area (when burr still red), or when it is already cold. The burr takes around 25cm to cool down from red.
 
You cannot avoid the burr by altering the welding essential variables because of the force used in HF welding to produce a sound joint. It has to be removed by mechanical methods or leave it alone.
 
Thanks metengr and EdStainless, I am already working on a device to remove it.
 
Does any of you know where can I get a tool to do this job? Any manufacturer of this kind of tool? Or who has seen mechanical methods to remore this burr in real industry?

Thanks a lot


 
Try the internet, these are usually called scarfing or skiving tools

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 