Chemical
Sep 8, 2009
4
Does any one know if we can remove Hydrogen and methane by the means of wet scrubber from Argon.
Thanks
 
Replies continue below

Recommended for you

I would guess that your best bet would be to raise the pressure up until the argon condensed and you could bleed off the liquid. The other choice would be a membrane but you would have to look around to find one for your application.

Regards
StoneCold
 
This would be a bit complex but you could take your gas stream and combust it. You'd get water and CO2 which you could remove in a pH controlled wet scrubber.
 
Since H2 boils at -430, CH4 -258 and Ar -302, seperating would be tough via cryogenics. Your best bet is mole sieves or a membrane.
 
Thank you all for your replies.
I am now looking at membrane separation for the purpose.
 