Is there any relationship between Ms(Martenstic start)temp & Grain sizes
Pandithan
 
While discussing the effect of grain size on Ms temperature, composition of the steel must be considered. Alloying elements have a strong role in influencing Ms temperature.

A few reports suggest that for a given alloy chemistry, with reduction in austenite grain size, there is a marginal dip in Ms temperature.

 