EngineerDave
Bioengineer
They say you learn something new everyday.
Today someone brought in a magnetic iron material. They stated that the grain size affects the magnetic properties.
I did some quick searches on this (found a girls presentation that was incomplete on this!), but was wondering if any of you knew off the top of your head what the general relationship is between grain size and magnetism in magnetic irons if there is any!
Today someone brought in a magnetic iron material. They stated that the grain size affects the magnetic properties.