We have having WPS with impact test at -29 Deg.c for FCAW process. as per ASME SEC-IX.
Now new filler wire brought having same SFA NO but different brand name from same manufacturer. Mechanical properties were same. Impact test carried out at -40 Deg.c
We need to qualify new PQR or Proceed with existing PQR.

Regards,
Shanmuga.
 
Not required per ASME IX, but may be by Buyer (Customer) specs.
 