Dear sir/all,
We have 2.5 KM of C.S. pipe line, and we have start the hydro test at 5pm with 18kg/cm2 and as per holding time of two hours , it is completed at 7pm , without any leakage or seepage.
But after completion of 2 hrs., pressure decrease by 1hrs. and it found 17kg/cm2.
We stated that due to decrease in temperatures, pressure also decrease. but client not ready to accept.
Pls help.
Design pressure is 12kg/cm2 and hydro test pressure is 18 kg/cm2.
(Sorry to members, wrongly posted in BPV forum, so posted in this, piping).
Regards
Prasad
We have 2.5 KM of C.S. pipe line, and we have start the hydro test at 5pm with 18kg/cm2 and as per holding time of two hours , it is completed at 7pm , without any leakage or seepage.
But after completion of 2 hrs., pressure decrease by 1hrs. and it found 17kg/cm2.
We stated that due to decrease in temperatures, pressure also decrease. but client not ready to accept.
Pls help.
Design pressure is 12kg/cm2 and hydro test pressure is 18 kg/cm2.
(Sorry to members, wrongly posted in BPV forum, so posted in this, piping).
Regards
Prasad