Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Recommended internal coating for pipeline that carries CO2 formation water

Status
Not open for further replies.

juancd200914

Petroleum
Joined
Mar 18, 2017
Messages
15
Location
EC
In a system of transport of water of formation in pipes of 4 in and 6 in, we have serious problems with the internal coating of the material, there has been blistering in the internal coating of the pipe, corrosion and erosion in fittings example 90 ° elbows , loss of material due to corrosion on the faces of the flanges and loss of material due to corrosion in the Oring, the internal coating of the pipe is TK505 and the coating on the accessories is Plasite 7159, I appreciate your help with references from companies that make internal coatings in pipeline or in turn with bibliography of the subject or documented cases.

Operations conditions:

Operation Pressure =2000 psi

Operation Temperature:220°F

Fluid: Formation Water with % od CO2

Pipe Material: API 5L X42 PSL2
FLANGE MATERIAL: ASTM A105
 