Dear Sirs,
Please give recommendation of bolting material considering followings.
1. Low strength bolting materials are limited to class 150 and class 300 in accordance with note 4 of table 1B in ASME B16.5.
Quote " These bolting materials may be used with all listed materials but are limited to Class 150 and Class 300 joints. See para. 5.3.4 for recommended gasket practices." unquote
2. ASTM A193 Grade B8MA, Class 1A is specified in Table 9 of NACE MR0103-2013 edition as material meeting the requirement of section 2.
SSC is mainly related to material strength and high hardness is main reason for susceptibility to SSC.
So, please give recommendation bolting material which meets the requirement of NACE MR0103 and is applied to 600# Class.
Thanks for your reply in advance.
Please give recommendation of bolting material considering followings.
1. Low strength bolting materials are limited to class 150 and class 300 in accordance with note 4 of table 1B in ASME B16.5.
Quote " These bolting materials may be used with all listed materials but are limited to Class 150 and Class 300 joints. See para. 5.3.4 for recommended gasket practices." unquote
2. ASTM A193 Grade B8MA, Class 1A is specified in Table 9 of NACE MR0103-2013 edition as material meeting the requirement of section 2.
SSC is mainly related to material strength and high hardness is main reason for susceptibility to SSC.
So, please give recommendation bolting material which meets the requirement of NACE MR0103 and is applied to 600# Class.
Thanks for your reply in advance.