Rebar Weld Size

Status
Not open for further replies.

Veer007

Civil/Environmental
Joined
Sep 7, 2016
Messages
379
Location
IN
Hey guys, i have to weld a 25mmØ rebar with 19mm thick bearing pate, is there any details for weld standard to develop its full shear and tensile capacity of rod? Also 19mmØ rebar. (FILLET WELD , ROD PERPENDICULAR TO PLATE)

Thanks in advance!!
 
The PCI manual has convenient design tables for this

 
You did not state the orientation of the rebar-to-plate. Here is PCI's info from their Handbook (7th Edition):

Capturepci2_ctrqaw.png
 
The rod perpendicular to plate, i need fillet weld size

Thanks in advance!!
 
PCI Handbook chapter 6 has these design aids:

Capturepci3_wdkfaq.png


A more legible part-image of above, for Grade 60:

Capturepci4_kzr23i.png
 