Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

rebar "material properties" Eurocode

Status
Not open for further replies.

monchie

Structural
Feb 22, 2011
96
Hello,

What is the right rebar "material properties" for Eurocode(ETABS 2015)?

At the moment, when I choose material properties for "rebar", the only option is "user".

If ever what is the right value for user define properties for rebar,if I wanted fy =500 MPa?

Any ideas/help is greatly appreciated.


Regards,
 
Replies continue below

Recommended for you

You need to check your local standards and select the appropriate properties for the reinforcement steel considered.

For B500B, you'd have:
Weight per Unit Volume: 77 kN/m3
E = 200E6 kPa
A = 1.17E-5 /ºC
Fy = Fye = 500E3 kPa
Fu = Fue = 500E3 x 1.08 = 540E3 kPa

Please check the following page:
 