Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

rebar "material properties" Eurocode

Status
Not open for further replies.

monchie

Structural
Joined
Feb 22, 2011
Messages
96
Location
IE
Hello,

What is the right rebar "material properties" for Eurocode(ETABS 2015)?

At the moment, when I choose material properties for "rebar", the only option is "user".

If ever what is the right value for user define properties for rebar,if I wanted fy =500 MPa?

Any ideas/help is greatly appreciated.


Regards,
 
You need to check your local standards and select the appropriate properties for the reinforcement steel considered.

For B500B, you'd have:
Weight per Unit Volume: 77 kN/m3
E = 200E6 kPa
A = 1.17E-5 /ºC
Fy = Fye = 500E3 kPa
Fu = Fue = 500E3 x 1.08 = 540E3 kPa

Please check the following page:
 