Rebar Lap Splice ACI 318-08

Status
Not open for further replies.

macan1

Structural
Joined
May 14, 2004
Messages
34
Location
CA
I am looking for rebar lap splice requirements in ACI 318-08 for concrete shear walls in seismic zone.
Could not find it.
Anyone can suggest?
 
A search for the word splice in chapter 21 of ACI 318-08 will reveal the main instances for the word, say...

21.1.6
21.1.7
21.4
21.5.2.3
21.5.2.4
21.8.2.(b)
21.9.2.3
21.9.6.5(b)
21.11.7.3
21.11.7.6
21.11.11.2

there may be more I have not annotated.
 