qualitypro
Mechanical
Pump shaft material is ASTM A240 S32760 and is damaged during operation. We have an approved weld procedure from the pump supplier. Can the shaft be repair welded and machined to bring it back to the original condition? Are there any precautions to be taken while welding duplex ss? or
Is it advisable to replace the shafts?