Aug 22, 2002 #1 Hugues Civil/Environmental Joined Mar 12, 2003 Messages 1 Location FR I would like to have some information on the reactivity of cumyl hydroperoxyde with hastelloy at concentration below 20% in demineralised water. I have the same question with ammonium persulfate in the same conditions
I would like to have some information on the reactivity of cumyl hydroperoxyde with hastelloy at concentration below 20% in demineralised water. I have the same question with ammonium persulfate in the same conditions
Aug 22, 2002 #2 mcguire Materials Joined Nov 2, 2001 Messages 1,086 Location US There is nothing in either of these compounds to pose any risk to hastelloy. For all practical purposes there will be no reaction at all. Upvote 0 Downvote
There is nothing in either of these compounds to pose any risk to hastelloy. For all practical purposes there will be no reaction at all.