I would like to have some information on the reactivity of cumyl hydroperoxyde with hastelloy at concentration below 20% in demineralised water.

I have the same question with ammonium persulfate in the same conditions
 
Replies continue below

Recommended for you

There is nothing in either of these compounds to pose any risk to hastelloy. For all practical purposes there will be no reaction at all.
 