Dear members,
Regarding the underwater welder qualification, I have a trouble in range of qualified thickness for fillet weld following AWS D3.6 (underwater welding). In this code mentioned 0.5t to 2t for groove weld only, not mentioned for fillet weld. Could you please inform me the range of qualified thickness for fillet weld following AWS D3.6(Thickness of test sample is 16mm).Thank you.
Regarding the underwater welder qualification, I have a trouble in range of qualified thickness for fillet weld following AWS D3.6 (underwater welding). In this code mentioned 0.5t to 2t for groove weld only, not mentioned for fillet weld. Could you please inform me the range of qualified thickness for fillet weld following AWS D3.6(Thickness of test sample is 16mm).Thank you.