Nov 14, 2016 #1 purode333 Mechanical Joined Sep 16, 2016 Messages 58 Location NG Dear sir, Which is commonly used electrode in rail welding. Rail CR 100 Regards Prasad
Nov 14, 2016 #2 kingnero Mechanical Joined Aug 15, 2009 Messages 1,783 Location BE joint welding or surfacing? What kind of rails? Vignole, grooved, craneway? Loads? You do realise that smaw joint welding is not a preferred choice? http://www.fusionpoint.behttp://be.linkedin.com/in/fusionpoint Upvote 0 Downvote
joint welding or surfacing? What kind of rails? Vignole, grooved, craneway? Loads? You do realise that smaw joint welding is not a preferred choice? http://www.fusionpoint.behttp://be.linkedin.com/in/fusionpoint
Nov 14, 2016 #3 berkshire New member Joined Jun 8, 2005 Messages 4,429 Location US For Railroad welding thermite is the preferred choice, It is quicker and cleaner. B.E. You are judged not by what you know, but by what you can do. https://www.youtube.com/watch?v=5uxsFglz2ig Upvote 0 Downvote
For Railroad welding thermite is the preferred choice, It is quicker and cleaner. B.E. You are judged not by what you know, but by what you can do.
Nov 16, 2016 #4 kingnero Mechanical Joined Aug 15, 2009 Messages 1,783 Location BE Agreed if you're talking maintenance joints, not when renewing rails on-site. Either way, if the question is about surface welding, this discussion is moot. http://www.fusionpoint.behttp://be.linkedin.com/in/fusionpoint Upvote 0 Downvote
Agreed if you're talking maintenance joints, not when renewing rails on-site. Either way, if the question is about surface welding, this discussion is moot. http://www.fusionpoint.behttp://be.linkedin.com/in/fusionpoint