Hi everyone,

I got some calculation sheet that explain how to determine radial stress from rubber material being compressed with axial pressure 'P' (see figure).
As far as I look around, I've never seen such formula like this, as I never dealing with rubber material before.
does anybody can enlight me where I can find some reference for this particular formula to let me have more understanding about this?

Thank you in advance

Yudhi
 
 http://files.engineering.com/getfile.aspx?folder=a8a56b05-1da6-42b6-8063-fba648e6451d&file=radial_formula.jpg
Google Poison's ratio. It is a property of all materials, including steel.
 
Hi Compositepro,

Thanks for the reponse.
Have you ever seen that formula? Do have have reference where the formula stated?
Im aware theat rubber poissons ratio is different from steel.

 
yes sure bro if their is any such formula exists
send me reference & it would be more better if you provide the Link
I m dealing in rubber business for last 25 Years , havent seen any thing like that before....

 