Hi experts,
I have two PQR'S
1) GTAW : Deposited weld metal 7mm
2) SMAW + GTAW : Deposited weld metal 70mm, GTAW (16mm), SMAW (54mm)
QUESTION : Can I make WPS Qualification ranges FROM 1.5 TO 200, Deposited weld metal GTAW(max 32mm), SMAW (max 200mm)?
AS PER QW200.2(f): yes
As per QW 200.4(b): No
Thanks
Brown
I have two PQR'S
1) GTAW : Deposited weld metal 7mm
2) SMAW + GTAW : Deposited weld metal 70mm, GTAW (16mm), SMAW (54mm)
QUESTION : Can I make WPS Qualification ranges FROM 1.5 TO 200, Deposited weld metal GTAW(max 32mm), SMAW (max 200mm)?
AS PER QW200.2(f): yes
As per QW 200.4(b): No
Thanks
Brown