Is there such a thing as a shelf-life for seamless 6061-T4 tubing? What about 6061-T6?
The diameter of the tubes in question is 2" and less and we store them indoors.
By shelf-life I mean a change in yield strength or hardness over time (6 months to years).
I have been unsuccessful in obtaining information from our tubing supplier.
Thanks in advance for any thoughts.