I have 20 or so (out of 7,000) anchor bolts (1" X 13" allthread) set in epoxy grout (17,000 psi avg strength) whose nuts are not fully engaged (about 1 to 2 threads below flush) Rather than bring in the core drillers to pull these out I would like to be able to have a welder come in and "kill" the nut - fill the opening of the nut with a puddle weld The nuts are 2H and they are in a horizontal plane splice connection They are spaced intermittently throughout a run of approximately 1600 feet AWS D1.1 allows the welding repair of anchor studs, but doesn't address this RCSC talks about load and welding with respect to rivets, but not this My PE has provided numbers indicating that there is little load involved (in fact, a jam nut could have been used instead of a full nut) Suggestions? Comments?