I am looking for some direction, I am looking for a rubber product with neoprene characteristics but with a relatively short hydrophilic reaction time. I need a robust material that will expand on contact with water within minutes.

I would appreciate any direction.
 
Replies continue below

Recommended for you

Hi
Those materials are around and used by the oil and gas industry under the term of Swellable elastomers, usually used in a product called swellable packers. they are conventional rubbers like NBR or HNBR to which has been added a very hydrophillic material which absorbs water and swells rapidly, usualy PVA (poly vinyl alcohol( not acetate !)if you are already in contact with a rubber compounder ask them about the above.if they are supplying the oil and gas industry they should know about them.
otherwise a search on Google with some of the above terms should point you in the right direction