I have a casting designated C35CrNiMo6.6. The parts made from these materials (relatively large block of 150x150x700 mm) show extreme poor mechanical properties, with yield and tensile almost equal, elongation <2% and Charpy-V values of average 7-8 J.
Can this material be heat treated (normalizing, followed by quench and teper perhaps) with negative effects such as grain-growth, or this is just "scrap"?
Can this material be heat treated (normalizing, followed by quench and teper perhaps) with negative effects such as grain-growth, or this is just "scrap"?