Hello, to all first time on here, seaming like a great information site.


I am looking for some general knowledge and personal experience on how to degrease stainless steel coils thickness of .015. Not only wondering information on how the process is down, and equipment manufacturers, but also maybe companies that outsource this type of work. Hope to get some help.


thanks in advance!
 
Lots of ways. Depends on where in the process you want to do it; we make wash stations.

I don't know the size of your coils, but my first thought is a ultrasonic was tank, with the proper solution.

Charlie
 
My first thought was electrolytic, but since have thought of ultrasonic. If have some time, please give me a call at 330-652-2501 and we can discuss this a little more. thanks
 