Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Query: Why is surface preparation (blasting) not allowed during night hours 1

Status
Not open for further replies.

mnthiraviam

Industrial
Joined
Apr 10, 2013
Messages
12
Location
AE
Query: Why is surface preparation (blasting) not allowed during night hours
 
What substrate?
Blasting with explosives?
Blasting with metal shot?
Blasting with abrasive media?
Where?
Who doesn't allow it? Which authority? Have you asked them?




Mike Halloran
Pembroke Pines, FL, USA
 
Because humidity increases at night because of lower temperature.
 
If you are talking about blasting steel, such as storage tanks or structures, the surface cools at night after sunset. As the sun rises, the air warms faster than the steel. The dew point of the air is higher than the temperature of the surfaceand the steel becomes a condensing surface for atmospheric moisture, causing flash rust, or interfering with coating performance or adhesion due to trapped moisture.