Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Query for requirement of HAZ impact specimen removal as per SEC VIII-Div I; UG84(g)(2)

Status
Not open for further replies.

amit217

Mechanical
Joined
Apr 16, 2013
Messages
5
Location
BH
I have one query regarding Impact specimen removal of HAZ as per SEC VIII-Div I UG84(g)(2).
Case – welded PQR with single side welded only one process. Base metal thickness is 8 mm. So question is can I prepare 7.5 mm thick impact specimen which is nearest obtainable thickness from 8 mm base metal ? Or as per fig.UG84.5 and Table UG84.6 – for base metal thickness ≤ 19 mm removal depth should be 1/4t to 1/2t, means I have to remove 2 mm(1/4t of 8mm) below the surface and prepare impact specimen 5 mm thick?
 
Prepare the largest specimen possible from the 8mm plate.
 