For welder performance qualification on "hard-facing overlay", QW-453 Note(8)(page 145 of Section IX 2007 edition) requires sectioning, macroetch and 5x visual examination of both surfaces. Inspection is for " cracks in base metal and HAZ, lack of fusion, or other linear defects"
How/where can I get a better definition of "other linear defects"? What about porosities? There must be a other guidelines that quantify linear indication size or clusters and other pass/fial criteria.
I'd also like to perfrom a cursory hardness checks on the welders test plates. QW-453 Note (7) says to take three hardness readings from locations shown in QW-462.5(e)(page 165 of Section IX 2007 edition) for plate coupons, but this figure is not revealing any location information. Can anyone clarify this please?
Thansk for any help.
How/where can I get a better definition of "other linear defects"? What about porosities? There must be a other guidelines that quantify linear indication size or clusters and other pass/fial criteria.
I'd also like to perfrom a cursory hardness checks on the welders test plates. QW-453 Note (7) says to take three hardness readings from locations shown in QW-462.5(e)(page 165 of Section IX 2007 edition) for plate coupons, but this figure is not revealing any location information. Can anyone clarify this please?
Thansk for any help.