mariocalvo
Materials
Dear all,
I have a dissimilar welding between P5A and P1. To carried out this joint, a buttering will be used. Our supplier has sent to us a PQR with the following steps:
1-P5A is buttered with E7018-A1 (up to 7mm after machining) and PWHT at 710ºC.
2-Weld the buttering to the P1 and PWHT at 620ºC.
The problem is that, the welding between P1 and the buttering, was done with 3 pass with GTAW (filler metal ER70S-6) and 1 pass with SMAW with E7018-A1. On the WPS the last pass will not be carried out.
Is that change allow by the code?
And on the other hand, the CS filler metal is alloyed with some Mo of E7018-A1 upgrading the mechanical properties of the weld, and this situation will not be done on production. I´am not sure if this PQR qualifies this joint and the WPS.
Thanks in advance.
I have a dissimilar welding between P5A and P1. To carried out this joint, a buttering will be used. Our supplier has sent to us a PQR with the following steps:
1-P5A is buttered with E7018-A1 (up to 7mm after machining) and PWHT at 710ºC.
2-Weld the buttering to the P1 and PWHT at 620ºC.
The problem is that, the welding between P1 and the buttering, was done with 3 pass with GTAW (filler metal ER70S-6) and 1 pass with SMAW with E7018-A1. On the WPS the last pass will not be carried out.
Is that change allow by the code?
And on the other hand, the CS filler metal is alloyed with some Mo of E7018-A1 upgrading the mechanical properties of the weld, and this situation will not be done on production. I´am not sure if this PQR qualifies this joint and the WPS.
Thanks in advance.