Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Pyrogel insulation thickness specificiation

Status
Not open for further replies.

ajcousins

Mechanical
Oct 28, 2021
6
Hello, I'm being asked to specify a thickness of pyrogel insulation on a vessel for heat conservation. Any ideas on how to go about doing this? The operating temp of the vessel is 250F.
 
Replies continue below

Recommended for you

How do you normally determine a thickness for a given insulation type? Pyrogel just had a smaller thermal conductivity that mineral wool, so it ends up being thinner.
 
How much heat conservation?

Our do you have a nominal thickness of rock wool.

If so the just pro rata that thickness looking at the heat transfer coefficients of the two.

HTC rock wool about 0.03 to 0.04 W/n/K
Aerogel about0.013.

So half the thickness of rock wool?