Hello all,
I have a question on the PWHT after welding for 15B30 materials. History: water quenched and tempered at 400F then welded.
My question is what is the correct PWHT temperature, read somewhere it should be lower than the initial tempering temperature and it makes sense as otherwise PWHT might cause unwanted microstructural change.
Cheers
I have a question on the PWHT after welding for 15B30 materials. History: water quenched and tempered at 400F then welded.
My question is what is the correct PWHT temperature, read somewhere it should be lower than the initial tempering temperature and it makes sense as otherwise PWHT might cause unwanted microstructural change.
Cheers