I am new to Vessel Industry and would like to know the differance between PHT and PWHT. I have a vessel that has PHT stamped on it and I wanted to know does it mean the entire vessel is Post Weld Heat Treated or just the portions of the vessel (like Nozzle...) is Heat Treated.
 
Replies continue below

Recommended for you

Partial Heat Treatment - only part of the vessel has been stress relieved.
 