According ASME 1 the minimum PWHT time for materials P15E (like SA-335 P91) with thickness over 5 inch is 5 hours.
For ASME B31.1 the minimum 5 hours is required already over 2 inch thickness.
Does anybody know why this difference or could this be a typo in B31.1?