I need to use two seperate PQR's for the welding on a P1 Low temp CS product. PWHT is req. due to the thickness. Impacts req. due to material.
PQR 1 has a pwht range of 625 - 635
PQR 2 has a pwht range of 600 - 620
As impacts are required QW407.2 states that a change in PWHT temperature and time range is a supplementary variable.
The way I see it I will have to conduct supplementary tests on PQR 2 using a PWHT range of 625 - 635? Could anybody clarify that this is the correct route to take. Or if there is any way around having to run supp. tests.
thanks.