The PWHT temperature specified for carbon steels ranges from 1100 F to 1200 F per ASME VIII. Some users have reported it necessary to use the 1175 F or higher PWHT temperature when the steel contains intentional additions of microalloying elements, such as Nb and V, in order to achieve HAZ hardness below 248 HV. I am talking about Carbon steel in wet H2S service.
Could any body here give me more information about this? Any papers recommended?
Could any body here give me more information about this? Any papers recommended?