Shall we PWHT SS TP 347H furnace tubes to be used in service of Hydrogen with partial pressure of 159 bar,H2S partial pressure of 1.4 x 10(-3)and vacuum gas oil?
PWHT heat up is 150/180ºC per hour, Four hour steep at 899ºC, and cool down at 150/180ºC per hour