Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

PWHT P-number 1 higher temperature 1

Status
Not open for further replies.

Jeldon

Chemical
Joined
May 20, 2013
Messages
25
Location
BR
What would be the highest PWHT temperature for the P-Number 1 according to TABLE UCS-56 of ASME SECTION VIII Div. 1

Kind regards
 
The highest temperature would be 1340 deg F, which corresponds to the approximate lower critical transformation temperature for P-No 1 base materials. The reason it is not listed as a maximum in Table UCS-56 is because Section IX requires re-qualification of a WPS with PWHT if the lower critical transformation temperature is exceeded.
 