I am working on horizontal tank fabricated in 1958.
the bottom half of the shell is monel 400 claded 1/8", base mareial 1.2" A212-B FBX. Now, I need add a new nozzle on it.
Question.
1. I only have ASME Code 1949, It looks like all welded PV had to perform PWHT at that time. Is here anybody have ASME 1958 to help me confirm if the vessel require PWHT due to mechanical reason. 1.2" CS did not require PWHT as per current Code.
2. The vessel is working in sour service. I beleive it is the process reason for PWHT. The new nozzle is located in claded area. Since the new nozzle did not direct contact process liquid. Can I avoid PWHT?
3. In case PWHT is required, If the PWHT will effect the corrosion resistance of the monel or break the bound between monel and CS?
Thanks
the bottom half of the shell is monel 400 claded 1/8", base mareial 1.2" A212-B FBX. Now, I need add a new nozzle on it.
Question.
1. I only have ASME Code 1949, It looks like all welded PV had to perform PWHT at that time. Is here anybody have ASME 1958 to help me confirm if the vessel require PWHT due to mechanical reason. 1.2" CS did not require PWHT as per current Code.
2. The vessel is working in sour service. I beleive it is the process reason for PWHT. The new nozzle is located in claded area. Since the new nozzle did not direct contact process liquid. Can I avoid PWHT?
3. In case PWHT is required, If the PWHT will effect the corrosion resistance of the monel or break the bound between monel and CS?
Thanks