Code: ASME VIII Div.1
Argument: a set-in joint, type figure UW-16.1(g), between a shell of SA 516 gr.70 and a LF2 forging nozzle.

Shell: SA 516 gr.70 plate thk.40mm
Nozzle: Forging with thickness in the large part 91,8mm

PWHT is required by ASME (UCS-56)
Table UCS-56 says that for the Nominal Thickness to use for the calculation of the minimum PWHT time you must see UW-40(f)
Question: What thickness should I use?
For UW-40(f)(5)(d) it should be 40mm, because I have no PAD, the attachment fillet weld is lower and the only weld is across the shell. Is it correct? Thanks
 
Replies continue below

Recommended for you

40mm is correct. Backed up by UW-40(f)(3) "for groove welds the nominal thickness is the depth of the groove". Groove is set through the shell 40mm.
Don't forget Full RT is mandatory for all Butt welds over 1-1/4" thick.
 
Don't forget Full RT is mandatory for all Butt welds over 1-1/4" thick.

david, did you mean to type 1-1/2"??
 