engineermat
Mechanical
ASME VIII Div.1 UCL-34(b)states that vessels or parts of vessels constructed of chromium stainless steel integral or weld metal overlay cladding and those lined with chromium stainless steel applied linings shall be postweld heat treated in all thicknesses.
Is this requirement applied to 304 austentic stainless steel?
Thanks.
Is this requirement applied to 304 austentic stainless steel?
Thanks.