We are quoting a replacement tube bundle for a high pressure steam generator (BKU), whose service clearly falls under UW-2(C) for unfired steam boilers. This bundle was already replaced once in 2014, and the tube-tubesheet joint at that time was strength welded but PWHT was not performed. The only welding that will take place on the replacement component is the tube-tubesheet weld.
What is your thoughts on this joint? Are we required to PWHT the tube-tubesheet joint in order to comply with UW-2(C)?
Thanks in advance.
We are quoting a replacement tube bundle for a high pressure steam generator (BKU), whose service clearly falls under UW-2(C) for unfired steam boilers. This bundle was already replaced once in 2014, and the tube-tubesheet joint at that time was strength welded but PWHT was not performed. The only welding that will take place on the replacement component is the tube-tubesheet weld.