Dear All,
We are procuring welded SA 403 fittings,During the review of WPS we found that PWHT (meniotned solution annealing as PWHT)is considered in WPS. As per SA 403 and Sec VIII div 1 , P8 material not required heat treatment ,unless design calculation say so.In our case there is no design requirement for PWHT.
So our doubt is ,can we consider material heat treatment as a PWHT in welded fittings ?
We are procuring welded SA 403 fittings,During the review of WPS we found that PWHT (meniotned solution annealing as PWHT)is considered in WPS. As per SA 403 and Sec VIII div 1 , P8 material not required heat treatment ,unless design calculation say so.In our case there is no design requirement for PWHT.
So our doubt is ,can we consider material heat treatment as a PWHT in welded fittings ?