Hello folks,
Attention please as the subject is not about basic issue of supplementary essential variables of ASME Sect. IX).
My sub-contractor submitted two WPS/PQR: The first WPS/PQR is for GTAW process without PWHT and the second is similar (all essential and no essential variables are the same) but with PWHT. (Knowing that charpy impact test is required for the project) He announced to use the WPS without PWHT but when production charpy impact test failed, he announced that he's gonna proceed with PWHT and that is cmpliant with the second WPS (with PWHT).
Do this comply with ASME sect. IX? Any interpretation would cover that behaviour? I would consider that as a fraud! but I will wait for your opinions
Thanks,
Attention please as the subject is not about basic issue of supplementary essential variables of ASME Sect. IX).
My sub-contractor submitted two WPS/PQR: The first WPS/PQR is for GTAW process without PWHT and the second is similar (all essential and no essential variables are the same) but with PWHT. (Knowing that charpy impact test is required for the project) He announced to use the WPS without PWHT but when production charpy impact test failed, he announced that he's gonna proceed with PWHT and that is cmpliant with the second WPS (with PWHT).
Do this comply with ASME sect. IX? Any interpretation would cover that behaviour? I would consider that as a fraud! but I will wait for your opinions
Thanks,