To All,
A.For ordering plate from the mill a Plate material specification is been issued.
B. One of the requirement for ordering is a PWHT coupon specifying the time and temperature it has to undergo .
1. For Item A - How would i know if the Plate material specification our engineering issued is correct?
How to check it against what?
2. For Item B - Where does the temperature and time came from? Let say temp = 607 C +/- 13 C and Time = 2.5hrs.
- How to determine the cycle needed?
I have made a PWHT procedure for 28mm thick holding time is 1 Hr and 8 minutes.
Thanks in advance
A.For ordering plate from the mill a Plate material specification is been issued.
B. One of the requirement for ordering is a PWHT coupon specifying the time and temperature it has to undergo .
1. For Item A - How would i know if the Plate material specification our engineering issued is correct?
How to check it against what?
2. For Item B - Where does the temperature and time came from? Let say temp = 607 C +/- 13 C and Time = 2.5hrs.
- How to determine the cycle needed?
I have made a PWHT procedure for 28mm thick holding time is 1 Hr and 8 minutes.
Thanks in advance