What are the deciding factor for PWHT ( coil or Band width ) requirement.


Some specs/ codes say 75 mm , some say 50 mm , some say 150 mm. So what are the basic criteria for selecting the Width of Induction Coil?
 
Replies continue below

Recommended for you

Thanks jones

D 10.10 really helpful

Thanks again
 