Jan 14, 2012 #1 nktqc Mechanical Joined May 10, 2011 Messages 37 Location AE What are the deciding factor for PWHT ( coil or Band width ) requirement. Some specs/ codes say 75 mm , some say 50 mm , some say 150 mm. So what are the basic criteria for selecting the Width of Induction Coil?
What are the deciding factor for PWHT ( coil or Band width ) requirement. Some specs/ codes say 75 mm , some say 50 mm , some say 150 mm. So what are the basic criteria for selecting the Width of Induction Coil?
Jan 14, 2012 #2 SJones Petroleum Joined Apr 22, 2001 Messages 3,948 Location GB The contractually specified requirements. If none are specified, then you can follow ISO 17663 or AWS D10.10 as appropriate and as seen fit. Steve Jones Materials & Corrosion Engineer http://www.linkedin.com/pub/8/83b/b04 Upvote 0 Downvote
The contractually specified requirements. If none are specified, then you can follow ISO 17663 or AWS D10.10 as appropriate and as seen fit. Steve Jones Materials & Corrosion Engineer http://www.linkedin.com/pub/8/83b/b04
Jan 14, 2012 Thread starter #3 nktqc Mechanical Joined May 10, 2011 Messages 37 Location AE Thanks jones D 10.10 really helpful Thanks again Upvote 0 Downvote