On a P1 to P1 pipe l, we have a weld to make on material with NWT of 1.375. Our WPS covers to basemetal thickness range of 1.875 to 9.00". The GTAW maximum is 1" and the SMAW maximum is 8". The WPS does not make mention of PWHT, permissible under Section IX, QW 407.1. However, under B31.1, Table 132 indicates that PWHT is required, only receiving exemption based on the carbon equivalent. We are trying to locate the MTRs, and will perform a PMI should our hunt be unsuccessful. Is this the correct approach? Am I looking at an essential variable here? I have not come up on this thickness and this situation in a P1 before, and the two codes seem to contradict each other to an extent. Thanks for any help.