Hello Everybody,

Do you know how to make out the specific test bench for the pure shear in rubber testing ?

Thaks for your help.
 
Replies continue below

Recommended for you

If one goes back to the mechanics, lap shear test is the "pure shear" test cited.

But is is not easy to make a good specemens.


I believe ASTM books talked about adhesive lap shear test.
 
Really "pure" shear tests are hard to arrange with rubber, but there is an ISO standard for a quadruple lap shear specimen you might consider. There was also a paper given on dynamic testing of rubber a few years ago that covered several kinds of specimens and test methods. You may find it by having the U of Akron library do a literature search; the author is still around and might be helpful as well.
 