ASTM D395 Compression Set Fixture is to test rubber, elastomer, silicone rubber and others compression set after compressed for certain period under constant strain at given temperature.

Sorted by different types of rubber, different thickness spacer rings should be adopted. The fixture should be made of stainless steel as this test may need to be done in high temperature and humidity environment.
 