Dear Gents,
I would like to ask for the acceptance criteria of pull off testing using dolly (Hydraulic Adhesion Tester)? We have applied primer, intermediate and top coat after we conduct pull off test after 2 weeks. The result of the pull off test is 5 MPA. Is this acceptable?